Publikace UTB
Repozitář publikační činnosti UTB

Micro-hardness and morphology of LDPE influenced by beta radiation

Repozitář DSpace/Manakin

Zobrazit minimální záznam


dc.title Micro-hardness and morphology of LDPE influenced by beta radiation en
dc.contributor.author Ovsík, Martin
dc.contributor.author Krátký, Petr
dc.contributor.author Maňas, David
dc.contributor.author Maňas, Miroslav
dc.contributor.author Staněk, Michal
dc.contributor.author Bednařík, Martin
dc.relation.ispartof Key Engineering Materials
dc.identifier.issn 1013-9826 Scopus Sources, Sherpa/RoMEO, JCR
dc.identifier.isbn 9783038350620
dc.date.issued 2014
utb.relation.volume 606
dc.citation.spage 253
dc.citation.epage 256
dc.event.title 10th International Conference on Local Mechanical Properties, LMP 2013
dc.event.location Kutná Hora
utb.event.state-en Czech Republic
utb.event.state-cs Česká republika
dc.event.sdate 2013-11-06
dc.event.edate 2013-11-08
dc.type conferenceObject
dc.language.iso en
dc.publisher Trans Tech Publications Ltd
dc.identifier.doi 10.4028/www.scientific.net/KEM.606.253
dc.relation.uri https://www.scientific.net/KEM.606.253
dc.subject Cross - linking en
dc.subject Depth Sensing Indentation en
dc.subject Irradiation en
dc.subject Micro-hardness en
dc.subject Polyethylene en
dc.description.abstract This article deals with the influence of different doses of Beta radiation to the structure and mico-mechanical properties of Low-density polyethylene (LDPE). Hard surface layers of polymer materials, especially LDPE, can be formed by radiation cross-linking by β - radiation with doses of 33, 66 and 99 kGy. Material properties created by β - radiation are measured by microhardness test using the DSI method (Depth Sensing Indentation). Individual radiation doses caused structural and micro-mechanical changes which have a significant effect on the final properties of the LDPE tested. The highest values of micro-mechanical properties were reached at radiation dose of 66 and 99 kGy, when the micro-hardness values increased by about 21%. The changes were examined and confirmed by X-ray diffraction. © (2014) Trans Tech Publications, Switzerland. en
utb.faculty Faculty of Technology
dc.identifier.uri http://hdl.handle.net/10563/1004638
utb.identifier.obdid 43871855
utb.identifier.scopus 2-s2.0-84898847983
utb.identifier.coden KEMAE
utb.source d-scopus
dc.date.accessioned 2015-06-04T12:54:38Z
dc.date.available 2015-06-04T12:54:38Z
utb.contributor.internalauthor Ovsík, Martin
utb.contributor.internalauthor Krátký, Petr
utb.contributor.internalauthor Maňas, David
utb.contributor.internalauthor Maňas, Miroslav
utb.contributor.internalauthor Staněk, Michal
utb.contributor.internalauthor Bednařík, Martin
Find Full text